The production process of water-jet interlining is quite mature in China. However, due to machine and human factors, some products with defective quality may be produced, such as pasting, discoloration, degumming, wrinkling, etc. In fact, for some problems , we all have corresponding remedies, you can take a look at them together.
Face-to-face issues
1. The fabric is thin and does not match the water-jet cloth - the rubber particles of the water-jet cloth are too large and too dense (a water-jet cloth can be used instead. Usually in this case, look for a water-jet cloth with sparse and smaller rubber particles, but it needs to be carried out Test whether the pulling force reaches the best effect).
2. The fabric matches the water-jet cloth but is still over the surface --- adjust the pressure, temperature and time of the press (improper operation).
Overcolor problem
1. The color of the water-spray cloth does not match the fabric itself - the fabric is thin and the color does not match the non-adhesive parts of the body after bonding (choose color matching lining).
2. When bonding, some fabrics may change color after high temperature and do not match the non-stick lining part (select the entire garment to be put into the bonding machine).
Degumming problem
1. The quality problem of the water spray cloth itself - the coating amount is not enough, the time is too long, and the rubber particles have no adhesion effect (choose to replace the water spray cloth).
2. The fabric does not match the water-spray cloth---replace the water-spray cloth with one that is easy to bond with the fabric.
3. The bonding conditions do not meet the requirements - test the conditions required for strong bonding and pressing.
Wrinkling problem
1. Improper operation during gluing, not placing them flatly, causing wrinkles. Place the cut pieces flatly and not bundle them to avoid problems.
2. If the shrinkage ratio of the fabric and the water-jet fabric are too different, you should choose one with a consistent shrinkage rate. Change the texture of the fabric or water-jet fabric and adopt bias cutting.
3. Problems with bonding machine equipment.
Blistering problem
1. Improper operation of three factors during bonding (mainly pressure, temperature and time).
2. The coating of the water spray cloth is uneven.
3. The shrinkage ratio of the fabric and the water-sprayed cloth are too different.
Choose one that matches the shrinkage ratio
Change the texture of the fabric or spray cloth and cut it on the bias.
The above are the problems that occur when fabrics are bonded to water-sprayed fabrics. When choosing water-sprayed fabrics, be sure to choose water-sprayed fabrics that are similar in color and shrinkage to the fabric. When problems occur, they must be corrected promptly to prevent excessive losses.